1.7139 | 16MnCrS5 |
1.7139 is a case hardening steel for steam boilers and turbines, shafts for higher temperature ranges
Composition:
%C | %Si | %Mn | %P | %S | Cr | Mo | Ni | other |
0,14-0,19 | 0,40 | 1,00-1,30 | 0,035 | 0,02-0,035 | 0,80-1,10 | – | – | – |
Hot working:
Forging temperature range: 1200-850℃
Note: Heat to 1200 ℃. Do not forge below 850.
Heat treatment:
Soft annealing | Heat treatment to obtain a certain structure | Heat treatment to obtain a certain tensile strength | Carburize | Core hardening | Surface hardening | Temper |
650-700 | 850-950 | 900-1000 | 900-950 | 850-880 | 810-840 | 170-210 |
Main application:
Gear and link components, bevels, plate- and cog wheels
Shape of product:
Round, flat, step shape, ring, disc, shaft, other shape depend on customer needs