1.6511 | 39NiCrMo4 |
1.6511 is a medium-carbon steel. This steel does not age hardened. Core properties of 1.6511 is produced by conventional quenching and tempering. Case hardness lower than the nickel-aluminum steel may be developed.
Composition:
%C | %Si | %Mn | %P | %S | Cr | Mo | Ni |
0.32-0.40 | Max 0.4 | 0.5-0.8 | Max 0.035 | Max 0.035 | 0.9-1.2 | 0.15-0.3 | 0.9-1.2 |
Hot working:
Forging temperature range: 1100-850℃
Note: Heat to 1200 ℃. Do not forge below 850.
Heat treatment:
Annealing ℃ | Normalizing ℃ | Hardening temperature | Tempering temperature ℃ |
790-845 | 845-900 | 830-855 | To desired hardness |
Main application:
Wire, and seamless mechanical tubing
Shape of product:
Round, flat, step shape, ring, disc other shape depend on customer needs