13KhFA(13ХФА) |
It is a lower structural steel. This softer steel is more ductile. This is one of general steel grade. It is used for Structural components and general purposes.
Composition:
C | Si | Mn | Ni | S | P | Cr | V | N | Al | Cu |
0.11 – 0.17 | 0.17 – 0.37 | 0.4 – 0.65 | max 0.25 | max 0.015 | max 0.015 | 0.5 – 0.7 | 0.04 – 0.09 | max 0.008 | 0.02 – 0.05 | max 0.25 |
Hot working:
Forging temperature range: 1240-850℃
Note: Heat to 1250 ℃. Do not forge below 850.
Heat treatment:
annealing ℃ | Normalizing ℃ | Hardening temperature for quenching in Water ℃ | Tempering temperature ℃ |
690-740 | 840-970 | 940-980 | 540-680 |
Main application:
Crankshafts, screws, bolts
Shape of product:
Round, flat, step shape, ring, disc, shaft, other shape depend on customer needs